Title:IZBOLJŠAVA RAZTRŽNIH VREDNOSTI STEKLENIH ARMATUR ZA OJAČANJE BRUSNIH IZDELKOV
Authors:ID Krajnik, Eva (Author)
ID Goršek, Andreja (Mentor) More about this mentor... New window
ID Pečar, Darja (Comentor)
ID Metličar, Marija (Comentor)
Files:.pdf MAG_Krajnik_Eva_2015.pdf (2,95 MB)
MD5: A85A239AEA9010365AE93D3653BD2977
 
Language:Slovenian
Work type:Master's thesis/paper
Typology:2.09 - Master's Thesis
Organization:FKKT - Faculty of Chemistry and Chemical Engineering
Abstract:Namen magistrskega dela je bil določiti vpliv staranja steklenih filamentov na raztržne vrednosti, ter vpliv reagentov za spajanje (silanov) na steklene filamente. Želeli smo primerjati raztržne vrednosti surovih in impregniranih filamentov različnih proizvajalcev, ugotoviti ali raztržne vrednosti v določenem časovnem območju začnejo izgubljati svoje vrednosti in primerjati končne rezultate po proizvajalcih in med njimi. Zanimal nas je tudi vpliv reagentov za spajanje na impregnirane steklene diske. Primerjali smo različne tipe reagentov za spajanje na različnih tipih niti. Preverili smo, ali lahko z njimi izboljšamo raztržne vrednosti impregnirane tkanine za bolj zahtevne kupce in ali imajo kakršenkoli vpliv na ostale parametre v fazi impregnacije. Glede na dobljene raztržne vrednosti surovih in impregniranih filamentov smo ugotovili, da se pri večini proizvajalcev pojavi vpliv staranja. Analize raztržnih vrednosti filamentov so pokazale, da pri nekaterih proizvajalcih le-te s časom močno padejo. Prav tako so se pokazale razlike v raztržnih vrednostih istih tipov steklenih filamentov različnih proizvajalcev. Z dodajanjem reagentov za spajanje smo dosegli do 12 % izboljšave raztržnih vrednosti v primerjavi s standardom. Ugotovili smo, da različni tipi reagentov za spajanje na steklenih filamnetih različnih proizvajalcev delujejo različno. Ne vplivajo pa na zahtevane parametre v samem procesu impregnacije.
Keywords:stekleni filamenti, raztržne vrednosti, staranje, reagenti za spajanje, fenolformaldehidna smola
Place of publishing:Maribor
Publisher:[E. Krajnik]
Year of publishing:2015
PID:20.500.12556/DKUM-47331 New window
UDC:661.727.1(043.2)
COBISS.SI-ID:18572054 New window
NUK URN:URN:SI:UM:DK:IAPSVXSO
Publication date in DKUM:30.03.2015
Views:1617
Downloads:125
Metadata:XML DC-XML DC-RDF
Categories:KTFMB - FKKT
:
Copy citation
  
Average score:(0 votes)
Your score:Voting is allowed only for logged in users.
Share:Bookmark and Share



Hover the mouse pointer over a document title to show the abstract or click on the title to get all document metadata.

Secondary language

Language:English
Title:TENSILE STRENGTH IMPROVEMENT ON GLASS ARMATURE FOR FURTHER ABRASIVE PRODUCTS RECOVERY
Abstract:The purpose of this master's work was to determine the influence of glass filaments aging on tensile strenght, and influence of silane coupling agent on glass filaments. We wanted to compere the results of tensile strenght on raw and impregnated glass filaments of different producers, to determine if they lose their values with time, and compare the final results between producers. We were also interested in the influence of silane coupling agents on impregnated glass disks. We compared different types of silane coupling agent on differenttypes of glass yarns. We checked, if they can help in improving the tensile strenght of the impregnated fabric for more demanding customers and if they have any impact on other parameters in the stage of impregnation. According to the results of the tensile strenght of raw and impregnated filaments, we found that at most producers influence of aging appear. Analysis of tensile strenght of the filaments have shown that for some producers thensile strenght with time fall sharply. They have also shown differences in the tensile strenght of the same types glass filaments of different producers. With the addition of silane coupling reagents around 12 % of tensile strenght improvement was achived compared with the standard. We found that different types of silane coupling agents on glass filaments shove different behaviour regarding producers. But they do not have any influence on parameters in impregnation process.
Keywords:fiberglass, tensile strenght, aging, silane coupling agent, formaldehyde resin


Comments

Leave comment

You must log in to leave a comment.

Comments (0)
0 - 0 / 0
 
There are no comments!

Back
Logos of partners University of Maribor University of Ljubljana University of Primorska University of Nova Gorica